I haven’t watched the video yet, but wow. That really shows the difference that heat makes on this project, rather than UV.
For followers that don’t follow my other doll-nerd...

dollsonmain:

elizabethplaid:

dollsonmain:

ooo 

\warning for blood

I haven’t watched the video yet, but wow. That really shows the difference that heat makes on this project, rather than UV.

For followers that don’t follow my other doll-nerd friends, the group has been discussing how to de-yellow vintage dolls. John (oak23, dolljunk) has been working on vintage Takara dolls, and Chris (dolldirt) posted his progress with a vintage Allan head.

He corrects himself later and says it’s not 40% peroxide, it’s 40 vol, which is 12%.